Defect characteristics: the appearance of the casting is incomplete,there are crack-like gaps or cut-offs,and the metal edges at the cracks or cut-o...
Our factory successfully used urea cores to make complex internal cavity parts...
The Investment Casting Market is poised to register a CAGR of 4.58% over the forecast period 2020 - 2025...
Dynamic balance...
Lost foam casting...
![]() |
Process
|
sodium silicate sand casting.
|
Specification
|
1.Material: stainless steel CF8,CF8M,CF3,CF3M,CF8C,CF20,CA-15,CA-40,etc.
2.Standard: ASTM\DIN\BS\JIS\GB.
3.Surface finish: acid clean,shot blasting,sand blasting, polishing,etc.
4.Weight: 1-7000kg.
|
Production facility
|
1.Casting facility:sand mixer,moulding machine, medium-frequency induction furnace,box resistance furnace, heat treatment furnace,shot-blasting machine,sand-blasting machine, .
2.Machining facility: CNC,NC lathe,ordinary machine tools.
|
Heat treatment
|
Solution Treatment.
|
Test facility
|
spectrometer,tensile test machine,hardness test machine,impact tester,CMM.
|